This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2017, 8, 1760–1768, doi:10.3762/bjnano.8.177
Figure 1: Representation of the applied cryogenic treatment.
Figure 2: Schematics of the used scratch method to measure friction and wear: (a) pre-scan to get the initial...
Figure 3: SEM image of a) CHT specimen and b) DCT specimen, showing a martenstic matrix with precipitated glo...
Figure 4: Elastic recovery values for nanoindentations performed with a conical indenter (r ≈ 100 µm) at 1000...
Figure 5: a) Evolution of wear coefficient during the tests at 1000 μN of applied normal load and b) cumulati...
Figure 6: Evolution of the relative average roughness after each test cycle.
Figure 7: Evolution of the friction coefficient during the nanowear test.
Figure 8: Scanning probe microscopy (SPM) image after 30 cycles of nanoscratch testing in a DCT specimen. The...
Figure 9: Depth profiles after a wear test in a DCT specimen in the a) longitudinal and b) transversal direct...